Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.00100 - 0.0100 GPa | 0.145 - 1.45 ksi | Youngs Modulus |
MarkeTech Silica Aerogel Silica aerogels are generally known for being an extremely lightweight transparent solid down to |
|||
Modulus of Elasticity | 0.00100 GPa | 0.145 ksi | |
Dow Corning JCR 6140 Two-part, transparent, medium modulus LED encapsulant with high transparency and medium viscosity.Information provided by Dow Corning |