Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 400 MPa | 58000 psi | |
LyondellBasell Lupolen® 5021 D HDPE, Blow Molding Grade Easy flow, blow molding grade for small containers (up to 5 l), bottles for surface-active substances, household chemicals, laundry and dishwashing detergents, sanitary cleaners, cosmetics and pharm.. |
|||
Tensile Creep Modulus, 1 hour | 400 MPa | 58000 psi | |
LyondellBasell Lupolen® 5261 Z HI HDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Creep Modulus, 1 hour | 400 MPa | 58000 psi | |
LyondellBasell Lupolen® 5261 ZS HDPE, Blow Molding Grade Relatively high viscosity blow molding grade (similar to Lupolen 5261 Z), but more resistant to stress cracking) for rigid, stackable and highly shock resistant containers for packaging all types of.. |
|||
Tensile Creep Modulus, 1 hour | 400 - 570 MPa | 58000 - 82700 psi | Average value: 465 MPa Grade Count:4 |
Overview of materials for High Density Polyethylene (HDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a.. |