Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 2600 MPa @Temperature 23.0 °C |
377000 psi @Temperature 73.4 °F |
ISO 899 |
DuPont Performance Polymers Crastin® FG6129 NC010 PBT
(Unverified Data**) Crastin® FG6129 NC010 is an unreinforced, high viscosity polybutylene terephthalate resin for extrusion and injection molding. It has been developed for consideration into applications such as part.. |
|||
Tensile Creep Modulus, 1 hour | 2600 MPa @Temperature 23.0 °C |
377000 psi @Temperature 73.4 °F |
ISO 899 |
DuPont Performance Polymers Crastin® S600F20 NC010 PBT
(Unverified Data**) Crastin® S600F20 NC010 is an unreinforced, lubricated, medium viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Creep Modulus, 1 hour | 2600 MPa @Temperature 23.0 °C |
377000 psi @Temperature 73.4 °F |
ISO 899 |
DuPont Performance Polymers Crastin® S600F40 NC010 PBT
(Unverified Data**) Crastin® S600F40 NC010 is an unreinforced, lubricated, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Creep Modulus, 1 hour | 2600 MPa | 377000 psi | |
Arkema Group Oroglas® MI-2T Acrylic
(discontinued **) OROGLAS MI-2T is an injection molding acrylic grade that offers excellent thermal resistance with slight improvement in impact performance.Key features improved deformation and toughness : up to 2.. |
|||
Tensile Creep Modulus, 1 hour | 2600 MPa | 377000 psi | ISO 899-1 |
Lanxess Durethan® BKV 115 H2.0 901510 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 15, even in.. |
|||
Tensile Creep Modulus, 1 hour | 2600 MPa | 377000 psi | ISO 899-1 |
Lanxess Durethan® BKV 115 000000 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 15, even in.. |
|||
Tensile Creep Modulus, 1 hour | 2600 MPa @Time 3600 sec |
377000 psi @Time 1.00 hour |
ISO 899-1 |
DuPont Performance Polymers Crastin® FG6129 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced High Viscosity Polybutylene Terephthalate Developed for Food Contact Applications and Extrusion and Injection Molding Crastin FG6129 NC010 is an unreinforced high viscosity polybutylene.. |
|||
Tensile Creep Modulus, 1 hour | 2600 MPa @Time 3600 sec |
377000 psi @Time 1.00 hour |
ISO 899-1 |
DuPont Performance Polymers Crastin® FGS600F10 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Polybutylene Terephthalate Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Creep Modulus, 1 hour | 2600 MPa @Time 3600 sec |
377000 psi @Time 1.00 hour |
ISO 899-1 |
DuPont Performance Polymers Crastin® FGS600F40 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Food Contact Applications Crastin FGS600F40 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for injection .. |
|||
Tensile Creep Modulus, 1 hour | 2600 MPa @Time 3600 sec |
377000 psi @Time 1.00 hour |
ISO 899-1 |
DuPont Performance Polymers Crastin® S600F40 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Low Viscosity Polybutylene Terephthalate Crastin S600F40 NC010 is an unreinforced lubricated low viscosity polybutylene terephthalate resin for injection molding.Information provided by.. |
|||
Tensile Creep Modulus, 1 hour | 2600 MPa @Time 3600 sec |
377000 psi @Time 1.00 hour |
ISO 899-1 |
DuPont Performance Polymers Crastin® S620F20 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S620F20 NC010 is an unreinforced nucleated lubricated medium viscosity polybutylene terephthalate resin for fast injection molding.In.. |
|||
Tensile Creep Modulus, 1 hour | 2600 MPa | 377000 psi | |
Arkema Group Oroglas® V 045 I Acrylic, Extrusion Grade
(discontinued **) OROGLAS V 045 I is an extrusion that exhibits the following properties : 50% tougher than standard acrylics excellent optical properties ( comparable to that of standard acrylics) superior surface .. |
|||
Tensile Creep Modulus, 1 hour | 2600 MPa | 377000 psi | |
Arkema Group Oroglas® VM Acrylic, Injection Molding Grade
(discontinued **) OROGLAS VM is an injection molding grade with a medium heat resistance and easy flow.OROGLAS VM is particularly suitable to improve mold filling of technical parts.The VM L version has been speciall.. |