Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 6900 MPa | 1.00e+6 psi | ISO 899-1 |
Lanxess Pocan® B 3225 000000 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding |
|||
Tensile Creep Modulus, 1 hour | 6900 MPa | 1.00e+6 psi | ISO 899-1 |
Lanxess Pocan® B 3225 901510 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding |