Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 1800 - 2200 MPa | 261000 - 319000 psi | Average value: 2080 MPa Grade Count:5 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Tensile Creep Modulus, 1 hour | 1600 - 2200 MPa | 232000 - 319000 psi | Average value: 1930 MPa Grade Count:3 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |