Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 455 MPa | 66000 psi | |
Covestro Desmopan® 372 Thermoplastic Polyurethane Desmopan 372 is a TPU on the basis of a special ester.Applications: Transport rolls, technical automotive parts.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separa.. |