Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 2700 MPa @Temperature 23.0 °C |
392000 psi @Temperature 73.4 °F |
ISO 899 |
DuPont Performance Polymers Delrin® 300PE NC010A Acetal Homopolymer Delrin® 300PE NC010A is a medium-high viscosity acetal homopolymer, an enhanced version with extremely low VOC emissions. It has improved processing thermal stability, good mechanical properties, a.. |
|||
Tensile Creep Modulus, 1 hour | 2700 MPa @Temperature 23.0 °C |
392000 psi @Temperature 73.4 °F |
ISO 899 |
DuPont Performance Polymers Delrin® 100PE NC010A Acetal Homopolymer Delrin® 100PE NC010A is a high viscosity acetal homopolymer, an enhanced version of Delrin® 100P with extremely low VOC emissions. It has improved processing thermal stability, good mechanical pro.. |
|||
Tensile Creep Modulus, 1 hour | 2700 MPa | 392000 psi | |
Arkema Group Orgalloy® RS 6015 EST Nylon 6 Alloy, 18% Glass Fiber (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties... |
|||
Tensile Creep Modulus, 1 hour | 2700 MPa | 392000 psi | |
Arkema Group Altuglas® GR 7E LIL Acrylic ALTUGLAS GR 7E LIL is an injection molding grade with excellent balance between mechanical, thermal and optical properties.Key features : easy processing and demolding improved chemical resistance .. |
|||
Tensile Creep Modulus, 1 hour | 2700 MPa | 392000 psi | |
Arkema Group Altuglas® 84 L Acrylic-Styrene Copolymer ALTUGLAS 84 L is a new type of acrylic polymer produced by ATOHAAS which increases the range of material for injection molding applications. ALTUGLAS 84 L is a styrene methylmethacrylate copolymer s.. |
|||
Tensile Creep Modulus, 1 hour | 2700 MPa | 392000 psi | |
Arkema Group Oroglas® V 044 Acrylic, Extrusion Grade
(discontinued **) OROGLAS V 044 is an extrusion grade offering good compromise between physical properties and thermal resistance.OROGLAS V 044 is recommended for extrusion of profiles, tubes and sheets.ISO data prov.. |
|||
Tensile Creep Modulus, 1 hour | 2700 MPa | 392000 psi | |
Arkema Group Oroglas® V 045 Acrylic, Extrusion Grade
(discontinued **) OROGLAS V 045 is a lubricated extrusion grade offering good combination of physical and optical properties.OROGLAS V 045 provides easy processing behavior.OROGLAS V 045 is recommended for extrusion.. |
|||
Tensile Creep Modulus, 1 hour | 2700 MPa | 392000 psi | |
Arkema Group Oroglas® V 825 HID Acrylic, UV, Heat Resistant
(discontinued **) OROGLAS HID is an acrylic resin formulated to withstand continuous exposure to high intensity discharge ( HID ) sources up to 90°c.Above 80°c, OROGLAS V 825 HID resin retains its original appearan.. |
|||
Tensile Creep Modulus, 1 hour | 2700 MPa | 392000 psi | |
Arkema Group Oroglas® V 825 T Acrylic
(discontinued **) OROGLAS V 825 T exhibits an excellent balance of properties including superior thermal resistance with an easy processing behavior.OROGLAS V 825 T is then the material of choice for automotive appli.. |
|||
Tensile Creep Modulus, 1 hour | 2700 MPa | 392000 psi | |
Arkema Group Oroglas® V 920 Acrylic, Injection Molding Grade
(discontinued **) OROGLAS V 920 is an injection molding grade with a good balance of properties :Superior flow with medium thermal resistance.The processing of OROGLAS V 920 is easy in terms of injection molding, mo.. |
|||
Tensile Creep Modulus, 1 hour | 2700 MPa | 392000 psi | |
Arkema Group Oroglas® V 920 T Acrylic, Injection Molding Grade
(discontinued **) OROGLAS V 920 T is an injection molding grade with an improved thermal resistance HDT A ( 1.82 MPa ) = 96°c without any adverse effect on mechanical and optical properties.The processing of OROGLAS.. |
|||
Tensile Creep Modulus, 1 hour | 2700 MPa @Temperature 23.0 °C |
392000 psi @Temperature 73.4 °F |
ISO 899 |
DuPont Performance Polymers Delrin® FG100P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG100P is a high viscosity acetal homopolymer, with improved thermal stability for use in easy to fill molds. It has been developed for consideration into applications such as parts for the.. |