Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 1900 MPa | 276000 psi | |
Covestro Bayblend® T 65 MN Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Interior automotive components.Information provided by Bayer.As of 1 September 2015,.. |
|||
Tensile Creep Modulus, 1 hour | 1900 MPa | 276000 psi | |
Arkema Group Oroglas® MI-7T Acrylic
(discontinued **) OROGLAS MI-7T is a medium impact grade combining excellent thermal resistance with good impact performance.Key features : impact resistance: up to 7 times more impact-resistant than standard acr.. |