Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 11000 MPa @Temperature 23.0 °C |
1.60e+6 psi @Temperature 73.4 °F |
50%RH; ISO 899 |
DuPont Performance Polymers Zytel® HTN 54G35HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN54G35HSLR NC010 is a 35% glass reinforced, toughened, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polym.. |
|||
Tensile Creep Modulus, 1 hour | 11000 MPa | 1.60e+6 psi | ISO 899-1 |
Lanxess Pocan® B 4235 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant |
|||
Tensile Creep Modulus, 1 hour | 11000 MPa | 1.60e+6 psi | ISO 899-1 |
Lanxess Pocan® BF 4235 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant |
|||
Tensile Creep Modulus, 1 hour | 11000 MPa @Time 3600 sec |
1.60e+6 psi @Time 1.00 hour |
50%RH; ISO 899-1 |
DuPont Performance Polymers Zytel® HTN 53G50LWSF BK702A Polyphthalamide (PPA)
(Unverified Data**) 50% Glass Reinforced High Performance Polyamide with Low Warpage and High Stiffness Information provided by DuPont Performance Polymers |
|||
Tensile Creep Modulus, 1 hour | 11000 MPa @Time 3600 sec |
1.60e+6 psi @Time 1.00 hour |
50%RH; ISO 899-1 |
DuPont Performance Polymers Zytel® HTN 54G35HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G35HSLR NC010 is a 35% glass reinforced toughened heat stabilized lubricated high performance polyamide resin. It is also a P.. |