Polymer Property : Tensile Impact Strength = 82.3 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 173 kJ/m²
82.3 ft-lb/in²
Kraton® D1102 + LDPE blend (10/90)
Blending KRATON D and G polymers with PE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A..