Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 140 kJ/m² | 66.6 ft-lb/in² | |
Solvay Specialty Polymers Kadel® E-1130 Polyketone
(discontinued **) High performance proprietary semi-crystalline polymer based resins with exceptional solvent resistance and high temperature performance. They provide strength and stiffness, plus superior chemical r.. |
|||
Tensile Impact Strength | 140 kJ/m² | 66.6 ft-lb/in² | |
Solvay Specialty Polymers Kadel® E-1230 Polyketone
(discontinued **) Electrical Conductor. High performance proprietary semi-crystalline polymer based resins with exceptional solvent resistance and high temperature performance. They provide strength and stiffness, p.. |
|||
Tensile Impact Strength | 140 kJ/m² | 66.6 ft-lb/in² | S Bar; ASTM D 1822 |
Chevron Phillips HiD® 9410 HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Wide Range of Processing Conditions, Good Parison Uniformity, Good TrimabilityApplications:Phar.. |
|||
Tensile Impact Strength | 140 kJ/m² | 66.6 ft-lb/in² | S Bar; ASTM D 1822 |
Chevron Phillips HiD® 9412/HiD® 9413 with Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding, Injection Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flo.. |
|||
Tensile Impact Strength | 140 kJ/m² | 66.6 ft-lb/in² | S Bar; ASTM D 1822 |
Chevron Phillips HiD® 99413F with Food Grade Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding, Injection Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flo.. |
|||
Tensile Impact Strength | 140 - 210 kJ/m² | 66.6 - 99.9 ft-lb/in² | Average value: 170 kJ/m² Grade Count:3 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Tensile Impact Strength | 140 kJ/m² | 66.6 ft-lb/in² | |
LyondellBasell Lupolen® 4152 D SW 00413 HDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |