Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 806 kJ/m² | 384 ft-lb/in² | ASTM D1822S |
Solvay Specialty Polymers Halar® 300 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |
|||
Tensile Impact Strength | 806 kJ/m² | 384 ft-lb/in² | ASTM D1822S |
Solvay Specialty Polymers Halar® 500 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |