Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 805 kJ/m² | 383 ft-lb/in² | 23°C; ASTM D-1822 |
ExxonMobil Escorene® LD-760 High EVA Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 27.5% vinyl acetate copolymer designed for specialty compounding applications. Excellent filler acceptance produces highly loaded concentrates.Ap.. |