Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 760 kJ/m² | 362 ft-lb/in² | 23°C; ASTM D-1822 |
ExxonMobil Escor® AT-320 EMAAA Terpolymer for Polymer Modification
(discontinued **) Data provided by the manufacturer, Exxon Chemical.45 Acid Number. Provides unusual adhesion to a variety of substrates and other components, such as aluminum foil, polyolefins, polycarbonate, PET, .. |
|||
Tensile Impact Strength | 760 kJ/m² | 362 ft-lb/in² | ASTM D1822S |
DuPont™ Surlyn® 9970 Ionomer Resin, Zinc
(discontinued **) Surlyn® 9970 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |