Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 550 kJ/m² | 262 ft-lb/in² | 23°C; ASTM D-1822 |
ExxonMobil Iotek® 7010 Zinc Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A zinc ionomer with excellent flexibility, abrasion resistance, impact strength and tensile strength. This ionomer has outstanding adhesion to glas.. |
|||
Tensile Impact Strength | 550 kJ/m² | 262 ft-lb/in² | 23°C; ASTM D-1822 |
ExxonMobil Iotek® 8020 Sodium Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A sodium ionomer with excellent abrasion resistance, impact strength, hardness and tensile strength. IOTEK ionomers provide superb low temperature .. |