Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 472 kJ/m² | 225 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HP2R PC Med/High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a.. |
|||
Tensile Impact Strength | 472 kJ/m² | 225 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HPS2 PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable.. |
|||
Tensile Impact Strength | 472 kJ/m² | 225 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HPS2 PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable.. |
|||
Tensile Impact Strength | 472 kJ/m² | 225 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® HPS2R PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable.. |
|||
Tensile Impact Strength | 472 kJ/m² | 225 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® LS1 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Automotive lens applications. Low viscosity. UV-stabilized. Transparent colors only. |
|||
Tensile Impact Strength | 472 kJ/m² | 225 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® LS1 PC (Asia Pacific) Automotive lens applications. Low viscosity. UV-stabilized. Transparent colors only. |
|||
Tensile Impact Strength | 472 kJ/m² | 225 ft-lb/in² | Type S; ASTM D 1822 |
SABIC Innovative Plastics Lexan® OQ2220 PC Ophthalmic/safety lens market. OQ2xxx series in all transparent tints. Dedicated equipment, stringent production control conditions.This data was supplied by SABIC-IP for the Americas region. |