Mechanical Properties Metric English Comments
Tensile Impact Strength 330 kJ/m²
157 ft-lb/in²
LyondellBasell Lupolen® 5261 Z HI HDPE
Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.