Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 273 kJ/m² | 130 ft-lb/in² | ASTM D1822 |
ExxonMobil HDPE HD 9830.02 High Density Polyethylene Resin Product Description: HD 9830.02 is a blow molding grade high density polyethylene copolymer with a bimodal molecular weight distribution. It provides a very good balance of stress crack resistance, .. |
|||
Tensile Impact Strength | 273 kJ/m² | 130 ft-lb/in² | Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S |
Dow 722 Linear Low Density Polyethylene (LDPE) DOW Polyethylene 722 is a broad molecular weight distribution homopolymer designed to offer good impact strength and rack resistance, with excellent flexibility. Typical applications include caps/c.. |