Polymer Property : Tensile Impact Strength = 480 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 80.0 - 480 kJ/m²
38.1 - 228 ft-lb/in²
Average value: 243 kJ/m² Grade Count:7
Overview of materials for High Density Polyethylene (HDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim..