Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 505 kJ/m² | 240 ft-lb/in² | At -20°C; ASTM D1822 |
DuPont Elvax® 460 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Tensile Impact Strength | 505 kJ/m² | 240 ft-lb/in² | At 23°C; ASTM D1822 |
DuPont Elvax® 660 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Tensile Impact Strength | 505 kJ/m² | 240 ft-lb/in² | At 23°C; ASTM D1822 |
DuPont Elvax® 550 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |