Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 504 kJ/m² | 240 ft-lb/in² | Long Specimen; ISO 179/1eA |
Aardvark Polymers Aarlon® 2000 Rotational Molding Resin, DAM Aarlon® 2000 PA 6/6 is a high performance nylon for rotational molding applications. Aarlon® 2000 offers high heat capabilities with exceptional mechanical properties.Information provided by G.. |
|||
Tensile Impact Strength | 504 kJ/m² | 240 ft-lb/in² | ASTM D1822 |
Formosa Plastics Formolene® HL3812 Film (Hexene) HDPE Medium Density Polyethylene Formolene® HL3812 is a high molecular weight hexene copolymer resin that is tailored specifically for geomembrane applications. The resin provides an excellent balance o.. |
|||
Tensile Impact Strength | 504 kJ/m² | 240 ft-lb/in² | ASTM D1822, Type S |
Dow AMPLIFY™ EA 103 Ethylene-ethyl Acrylate (EEA) AMPLIFY™ EA 103 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility and imparts low temperature toughness to a wide range of engineering resins. It can be ut.. |
|||
Tensile Impact Strength | 504 kJ/m² | 240 ft-lb/in² | Long Specimen; ISO 179/1eA |
Aardvark Polymers Aarlon® 2000 Rotational Molding Resin, 50% RH Aarlon® 2000 PA 6/6 is a high performance nylon for rotational molding applications. Aarlon® 2000 offers high heat capabilities with exceptional mechanical properties.Information provided by Gehri.. |