Polymer Property : Tensile Impact Strength = 135 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 135 kJ/m²
64.2 ft-lb/in²
S bar; ASTM D 1822
Chevron Phillips HiD® 9502H - 9503H High Performance Series HDPE Blow Molding Resin  (discontinued **)
Resin Type: linear copolymerCharacteristics: outstanding ESCR, excellent impact resistance, medium molecular weight distribution, wide range of processing conditions, high melt strength, good pariso..
Tensile Impact Strength 135 kJ/m²

@Temperature -30.0 °C
64.2 ft-lb/in²

@Temperature -22.0 °F
ISO 8256
Iran Petrochemical (PCC) HB5510 High Density Polyethylene
HB-5510 is a high molecular weight high density polyethylene.Applications: extrusion large blow moldings, jerry cans, film and blown bags.Information provided by Iran Petrochemical Commercial Co.
Tensile Impact Strength 135 kJ/m²
64.2 ft-lb/in²
S bar; ASTM D 1822
Chevron Phillips Marlex® 9503HF High Performance Series HDPE Blow Molding Resin
Resin Type: linear copolymerCharacteristics: outstanding ESCR, excellent impact resistance, medium molecular weight distribution, wide range of processing conditions, high melt strength, good pariso..