Mechanical Properties Metric English Comments
100% Modulus 0.00150 - 0.00170 GPa
0.218 - 0.247 ksi
DIN 53504 S2
Wacker Silicones Geniomer® 200 Silicone TPE Elastomer
SLM TPSE 200 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas..