Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.02059 GPa | 2.987 ksi | ASTM D638 |
SK Chemicals SKYTHANE® UB601 Ink Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta.. |