Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.01764 GPa | 2.559 ksi | JIS K6301 |
Stellarchem 8075 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
100% Modulus | 0.01764 GPa | 2.559 ksi | JIS K6301 |
Stellarchem AB760LG TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
100% Modulus | 0.01764 GPa | 2.559 ksi | JIS K6301 |
Stellarchem AB-860LG TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |