Polymer Property : 100% Modulus = 2.47 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.0170 GPa
2.47 ksi
ASTM D412
Lubrizol Advanced Materials PEARLCOAT® Activa D126K BL Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLCOAT® Activa D126K BL is a standard polyester based TPU, supplied in form of translucent, black colored pellets, combining hardness with excellent low-temperature flexibility. PEARLCOAT® Acti..
100% Modulus 0.0170 GPa
2.47 ksi
ISO 37
Huntsman AVALON® 60 DE Thermoplastic Polyurethane
Introduction: AVALON 60 DE is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 DE is part of the AVALON Perform Range and offers a premium soling materi..
100% Modulus 0.0170 GPa
2.47 ksi
ISO 37
Huntsman AVALON® 98 AB Thermoplastic Polyurethane
Introduction: AVALON 98 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 98 AB is part of the AVALON Performance Range and offers a premium soling ma..
100% Modulus 0.0170 GPa
2.47 ksi
DIN 53504
Huntsman IROGRAN® A 98 E 4735 Polyester-Based TPU-Injection Extrusion Grade
High Hydrolysis resistance and good crystallinity. Suggested for extrusion.Information provided by Huntsman
100% Modulus 0.0170 GPa
2.47 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-1198 Polyester Based TPU
Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd.
100% Modulus 0.0170 GPa
2.47 ksi
ISO 37
Lubrizol ESTANE® GP55DT Ether Based Thermoplastic Polyurethane
Type: Estane® GP 55DT is an aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tagsAvailable in ..
100% Modulus 0.0170 GPa
2.47 ksi
ISO 37
Lubrizol ESTANE® GP98AE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 98AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..