Polymer Property : 100% Modulus = 2.45 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.0169 GPa
2.45 ksi
ASTM D412
DuPont Performance Polymers Kalrez® 3018 FFKM Perfluoroelastomer  (discontinued **)
A carbon black-filled compound that is similar to Compound 1050LF, except for higher hardness/modulus. Best hot water/steam resistance. Generally used in oil fields and process industry application..