Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.01302 GPa | 1.889 ksi | ASTM D412 |
Lubrizol Advanced Materials PEARLCOAT® 126K Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLCOAT® 126K is a polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and medium softening point. PEARLCOAT® 1.. |