Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0112 GPa | 1.63 ksi | ASTM D-638 |
Axiall 38900 Wire & Cable Flexible PVC Low cost AWM jacket for SPT, SVT, SJT applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |