Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00931 GPa | 1.35 ksi | ASTM D412 |
S&E Specialty Polymers GA-2190E-FR CLEAR PVC Application: Specialty clear, 60° C insulating compound designed for excellent clarity and sunlight resistance.Information provided by S&E Specialty Polymers |
|||
100% Modulus | 0.00931 GPa | 1.35 ksi | ASTM D412 |
S&E Specialty Polymers TufTech™ GA-7056-1002 PVC Compound Application: A 75°C Jacketing Compound UL approved for 720 hr. sunlight resistance. Suitable for use in direct burial applications.Information provided by S&E Specialty Polymers |
|||
100% Modulus | 0.00930 GPa | 1.35 ksi | ASTM D412 |
Precision Polymer Engineering Perlast® G70H Perfluoroelastomer Special, pure white compound with high temperature properties and wide chemical resistance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing p.. |
|||
100% Modulus | 0.00931 GPa | 1.35 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00931 GPa | 1.35 ksi | |
Spartech E65080 General Purpose PVC First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B.. |
|||
100% Modulus | 0.00931 GPa | 1.35 ksi | ASTM D412 |
Teknor Apex UNIPRENE® 7100-40D Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
100% Modulus | 0.00931 GPa | 1.35 ksi | 500 mm/min; ASTM D 412 |
Zylog Neoplast® 180 HOFR Thermoplastic Vulcanizate Neoplast 180 HOFR is a flame retardant thermoplastic vulcanizate (TPV) compound, based on polyolefin chemistry, suitable for Injection Molding and Extrusion applications.RoHS Compliant, UV Stabilize.. |
|||
100% Modulus | 0.00931 GPa | 1.35 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00931 GPa | 1.35 ksi | ASTM D-638 |
Axiall 8852 Moldings & Extrusions Flexible PVC General purpose compound recommended for extrusion applications. Contains a biocide and is UV stabilized.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00931 GPa | 1.35 ksi | ASTM D-638 |
Axiall EX1188B Wire & Cable Flexible PVC UL 360 jacket compound. 105°C air; 60°C oil.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00930 GPa | 1.35 ksi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 4139D Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4139D is a high hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
100% Modulus | 0.00930 GPa | 1.35 ksi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 4439D Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4439D is a high hardness grade possessing exceptional tensile strength, superior compression s.. |