Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00900 GPa | 1.31 ksi | ISO 37 |
Termopol Termoton® V2GA1050d TPV Compound Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;.. |
|||
100% Modulus | 0.00900 GPa | 1.31 ksi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials Pearlthane® ECO D12T90 Thermoplastic Polyurethane Type : Pearlthane® ECO D12T90 is a high performance bio-based thermoplastic polyurethane. With ca. 38% bio-based content.Main Application : Injection MouldingSpecial Features : Very good flexibil.. |
|||
100% Modulus | 0.00900 GPa | 1.31 ksi | ISO 37 |
Huntsman AVALON® 92 AE Thermoplastic Polyurethane Introduction: AVALON 92 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 92 AE is part of the AVALON Perform Range and offers a premium soiling materi.. |
|||
100% Modulus | 0.00900 GPa | 1.31 ksi | DIN 53504 |
Lubrizol ESTANE® T4065 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.00900 GPa | 1.31 ksi | DIN 53504 |
Lubrizol ESTANE® X4928 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.00900 GPa | 1.31 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1190 Polyester Based TPU Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.00900 GPa | 1.31 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-8290 Polyether-Based TPU Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.00900 GPa | 1.31 ksi | ASTM D412 |
Lubrizol ESTANE® 58134 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUses: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |
|||
100% Modulus | 0.00900 GPa | 1.31 ksi | ASTM D412 |
Lubrizol ESTANE® 58219 Ether Based Thermoplastic Polyurethane Features: Excellent physical properties, hydrolysis resistance, low temperature performance and clarity. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection .. |
|||
100% Modulus | 0.00900 GPa | 1.31 ksi | ASTM D412 |
Lubrizol ESTANE® 58810 Ether Based Thermoplastic Polyurethane Features: High melt flow and improved temperature resistanceUses: Extrusion – Wire and cable, Hose and tubeAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by .. |
|||
100% Modulus | 0.00900 GPa | 1.31 ksi | ISO 37 |
Lubrizol ESTANE® GP92AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 92AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
100% Modulus | 0.00900 GPa | 1.31 ksi | ASTM D638 |
ELASTO UK Dryflex® 420401S SBS Based Material, 40D Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
100% Modulus | 0.00900 GPa | 1.31 ksi | ASTM D638 |
ELASTO UK Dryflex® 422401S SBS Based Material, 40D Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
100% Modulus | 0.00903 GPa | 1.31 ksi | ASTM D638 |
Colorite Polymers 8033 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00903 GPa | 1.31 ksi | ASTM D638 |
Colorite Polymers 8033SF General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00904 GPa | 1.31 ksi | |
C.O.I.M. PLAXTER® P 72 Polymeric Plasticizer Description: Formulated with PVC, it is used in the field of conveyor belt manufacturing as well as in the field of synthetic leathers.Information provided by P.A.T. Products, Inc. |
|||
100% Modulus | 0.00906 GPa | 1.31 ksi | |
C.O.I.M. PLAXTER® P 90 Polymeric Plasticizer Description: Formulated with PVC, it is used in the field of synthetic leathers.Information provided by P.A.T. Products, Inc. |
|||
100% Modulus | 0.00900 GPa | 1.31 ksi | |
ACC EP Primer 59 EPI Engineered Polymer EP Primer 59, “Powered by Reactamine® Technology”, is an ultra-fine, solvent-free Styrene modified acrylic-methacrylic-ester copolymer emulsion. It is suitable for both interior and exterior appl.. |
|||
100% Modulus | 0.00900 GPa | 1.31 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1695AB Polyester Based TPU Stable melt viscosity, outstanding toughness & tear resistance, good workability for high frequency weldingInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.00900 GPa | 1.31 ksi | ASTM D412 |
Lubrizol Estane® 2103-90AENH Film Grade Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: NSF Standard 61 Certified, FDA ComplianceAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane prod.. |
|||
100% Modulus | 0.00900 GPa | 1.31 ksi | ASTM D412 |
Lubrizol ESTANE® 58215 Ether Based Thermoplastic Polyurethane Features: Excellent physical properties, hydrolysis resistance and improved temperature resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and b.. |