Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.008791 GPa | 1.275 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.008791 GPa | 1.275 ksi | ASTM D-638 |
Axiall 13820 Wire & Cable Flexible PVC Non-lead stabilized, 720 hour sunlight resistant insulation compound recommended for TW and 75C Class 43 applications. Good low temperature performance. Also suitable for outdoor jacket applicatio.. |
|||
100% Modulus | 0.008791 GPa | 1.275 ksi | ASTM D-638 |
Axiall 13821 Wire & Cable Flexible PVC Non-lead stabilized, 720 hour sunlight resistant, TW insulation compound also recommended for 75C Class 43 applications or outdoor jacket applications.Information provided by Georgia GulfGeorgia Gul.. |
|||
100% Modulus | 0.008791 GPa | 1.275 ksi | ASTM D-638 |
Axiall 8810 Moldings & Extrusions Flexible PVC Low gravity extrusion compound especially formulated for extruded T-moldings and other shapes where uniform flow through the die is required. Exhibits good flex whitening resistance.Information pro.. |
|||
100% Modulus | 0.008791 GPa | 1.275 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |