Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00850 GPa | 1.23 ksi | 0.025" extruded film; DIN 53504 |
Huntsman IROGRAN® A 75 P 4655 N TPU-Polyester Introduction: IROGRAN A 75 P 4655 N is a black colored polyether based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 75 P 4655 N is a part of the HUNTSMAN injecti.. |
|||
100% Modulus | 0.00850 GPa | 1.23 ksi | Injection molded parts; DIN 53504 |
Huntsman IROGRAN® A 92 E 4670 TPU-Polyester Introduction IROGRAN A 92 E 4670 is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion/injection molding product range and offers a spe.. |
|||
100% Modulus | 0.00848 GPa | 1.23 ksi | ASTM D-638 |
Axiall 8864 Moldings & Extrusions Flexible PVC General purpose PVC extrusion compound recommended for applications that require UV and fungus resistance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00850 GPa | 1.23 ksi | |
Lubrizol Estane® 54601 Thermoplastic Polyurethane Feature: Produces high coating weight in one pass at high production speed. Broad process window and transparent spherical pellets.Uses: Melt roll coated fabrics and unsupported foilsAvailable in A.. |
|||
100% Modulus | 0.00848 GPa | 1.23 ksi | ASTM D412; ISO 37 |
Advanced Polymer Alloys Alcryn® 2095 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |