Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00740 GPa | 1.07 ksi | ASTM D412 |
Precision Polymer Engineering Perlast® G60T Perfluoroelastomer A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: This grade is particularly suited to static ap.. |
|||
100% Modulus | 0.00740 GPa | 1.07 ksi | ISO 37 |
Termopol Termoton® K2GA5080A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
100% Modulus | 0.00740 GPa | 1.07 ksi | |
Taiwan PU Corporation TPU-BH95 Hydrolysis Resistance, Blow Molding Polyether Base TPU Thermoplastic Polyurethane (TPU), Hydrolysis Resistance, Polyether Base, Blow MoldingInformation provided by Taiwan PU Corporation. |
|||
100% Modulus | 0.00740 GPa | 1.07 ksi | |
Taiwan PU Corporation TPUI-G90 High Wear Resistance, Injection Molding Polycaprolactone Base TPU Thermoplastic Polyurethane (TPU), High Wear Resistance, Polycaprolactone Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
100% Modulus | 0.00738 GPa | 1.07 ksi | |
Taiwan Sheen Soon Sheenthane® A8521 TPU for Ink Thermoplastic polyurethane elastomer for ink. Hydrolysis resistance gradeAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen.. |
|||
100% Modulus | 0.00738 GPa | 1.07 ksi | |
Taiwan Sheen Soon Sheenthane® A8521H TPU for Ink Thermoplastic polyurethane elastomer for ink. Hydrolysis resistance gradeAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen.. |
|||
100% Modulus | 0.00738 GPa | 1.07 ksi | 500 mm/min; ASTM D 412 |
Zylog Neoplast® 180 FT EB Thermoplastic Vulcanizate Neoplast 180 FT EB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.Ro.. |
|||
100% Modulus | 0.00740 GPa | 1.07 ksi | Press-cured 5 minutes at 190°C |
DuPont Vamac® DP Activator OC Coagent Test Compound Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper.. |
|||
100% Modulus | 0.00740 - 0.0113 GPa | 1.07 - 1.64 ksi | |
Zeon Chemicals Nipol® 1082V Polyblend Nitrile Elastomer Nipol® nitrile elastomers are recommended when oil or solvent resistance is needed for the proper functioning of rubber parts. Fuel, oil and solvent resistance improves as acrylonitrile content is .. |
|||
100% Modulus | 0.00740 GPa | 1.07 ksi | ASTM D412 |
Teknor Apex Sarlink® 4339D Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4339D is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set .. |