Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00720 GPa | 1.04 ksi | -10% change after 72 hours @ 260°C; ASTM D412 |
Precision Polymer Engineering Perlast® G60H Perfluoroelastomer Special, pure white compound with excellent high temperature properties and wide chemical resistance. Extremely low outgassing properties.Applications: For use in applications which require exposur.. |
|||
100% Modulus | 0.00720 GPa | 1.04 ksi | DIN 53504 |
Huntsman IROGRAN® A 92 E 4246 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 92 E 4246 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
100% Modulus | 0.00720 GPa | 1.04 ksi | ASTM D412 |
DuPont Vamac® DP Test Compound Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper.. |
|||
100% Modulus | 0.00720 GPa | 1.04 ksi | ASTM D412 |
DuPont Performance Polymers Kalrez® 6375UP FFKM Perfluoroelastomer Resists chemical attack and is formulated and processed to minimize the potential for undesirable contaminants. Kalrez® 6375UP has the best balance of performance characteristics required for semic.. |
|||
100% Modulus | 0.00720 GPa | 1.04 ksi | 500 mm/min; ASTM D412 |
DuPont Performance Polymers Kalrez® 6375 FFKM Perfluoroelastomer Kalrez Spectrum 6375, designed specifically for the chemical process industry, combines new polymer technology with innovative patented curing technology. Compound 6375 is designed to give outstandi.. |
|||
100% Modulus | 0.00717 GPa | 1.04 ksi | ASTM D-638 |
Axiall 801-83 Moldings & Extrusions Flexible PVC High temperature automotive harness tape.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00720 GPa | 1.04 ksi | ASTM D412 |
DuPont Performance Polymers Kalrez® 4079 FFKM Perfluoroelastomer A low compression set compound for general-purpose use in O-rings, diaphragms, seals, and other parts used in the process and aircraft industries. It is a carbon black-filled compound with excellen.. |