100% Modulus 0.00670 GPa
0.972 ksi
Die C; Cross direction; ASTM D412
Teknor Apex Sarlink® 4190 Thermoplastic Elastomer
A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4190 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical..
100% Modulus 0.00670 GPa
0.972 ksi
Die C; Cross direction; ASTM D412
Teknor Apex Sarlink® 4490 Thermoplastic Elastomer
A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4490 is a medium hardness grade possessing exceptional tensile strength, superior compressio..
100% Modulus 0.00670 GPa
0.972 ksi
Cured 10 minutes at 180°C
DuPont Vamac® DP 4.5 phr Peroxide Test Compound
Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper..
100% Modulus 0.00670 GPa

@Temperature 23.0 °C
0.972 ksi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 12 mil - Black, Shelf
Lubrizol Estane® 58610 Thermoplastic Polyurethane
Features: Combines flexibility, toughness and excellent roll release for calendering and melt coating applications.Uses: Injection molding and general extrusion techniques. It is used in film, shee..
100% Modulus 0.00670 GPa
0.972 ksi
Press Cure 7 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FC 2230 Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FC 2230 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul..
100% Modulus 0.00670 GPa
0.972 ksi
Cured 7 min at 177°C and Post Cured 16 hr at 232°C
DuPont Performance Polymers GLT305 Peroxide Cured Fluoroelastomer (FKM) Formulation  (discontinued **)
FormulationViton® GLT305