Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00527 GPa | 0.765 ksi | ASTM D412 |
SK Chemicals SKYTHANE® R180A Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
100% Modulus | 0.00527 GPa | 0.765 ksi | ASTM D638 |