Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00517 GPa | 0.750 ksi | ASTM D412 |
Teknor Apex UNIPRENE® 7100-80 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
100% Modulus | 0.00517 GPa | 0.750 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N330 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00517 GPa | 0.750 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00517 GPa | 0.750 ksi | ASTM D412 |
Elastocon TPE Technologies Elastocon® 8078N Thermoplastic Elastomer Elastocon® 8078N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8078N is FDA compliant and well suited.. |
|||
100% Modulus | 0.00517 GPa | 0.750 ksi | ASTM D412 |
DuPont Performance Polymers Kalrez® Spectrum™ 0040 Fluoroelastomer Kalrez® Spectrum™ 0040 perfluoroelastomer parts are specifically designed for low-temperature environments where significant chemical resistance is required. Proprietary polymer and cure technolog.. |
|||
100% Modulus | 0.00517 GPa | 0.750 ksi | |
Colorite Polymers Flexchem 6051-02 Vinyl Compound Description: The Flexchem "51" series is a group of translucent, flexible, non-toxic vinyl compounds which were specifically developed to replace silicone in various applications. These compounds ut.. |
|||
100% Modulus | 0.00517 GPa | 0.750 ksi | ASTM D-638 |
Axiall 8700 Moldings & Extrusions Flexible PVC General purpose, matte-finish extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00517 GPa | 0.750 ksi | Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FT 2320 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FT 2320 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |
|||
100% Modulus | 0.00517 GPa | 0.750 ksi | ASTM D-638 |
Axiall 1601 Clear 7002 Flexible PVC Flexible polyvinyl chloride compound formulated for USP Class VI applications. The compound possesses exceptional clarity.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation .. |
|||
100% Modulus | 0.00517 GPa | 0.750 ksi | ASTM D-638 |
Axiall 18753 Wire & Cable Flexible PVC Non-lead stabilized, fungus resistant 105 C rated jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00517 GPa | 0.750 ksi | ASTM D-638 |
Axiall 6652 Moldings & Extrusions Flexible PVC General purpose clear molding and extrusion compound with good processing characteristics and good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporati.. |
|||
100% Modulus | 0.00517 GPa | 0.750 ksi | ASTM D-638 |
Axiall 8730 Moldings & Extrusions Flexible PVC A high quality, profile extrusion compound recommended for those applications where exceptional low temperature performance is required.Information provided by Georgia GulfGeorgia Gulf became Axiall.. |
|||
100% Modulus | 0.00517 GPa | 0.750 ksi | ASTM D-638 |
Axiall 8747 Moldings & Extrusions Flexible PVC Economical general purpose molding and extrusion compound with good flex whitening resistance especially in darker colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation i.. |
|||
100% Modulus | 0.00517 GPa | 0.750 ksi | ASTM D-638 |
Axiall 10701 Wire & Cable Flexible PVC General purpose 80°C compound with good low temperature properties recommended for 15 mil wall and larger.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00517 GPa | 0.750 ksi | ASTM D638 |
Colorite Polymers 6575 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00517 GPa | 0.750 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N330 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00517 GPa | 0.750 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |