Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00490 GPa | 0.710 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 70 PHR N990 (MT) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00490 GPa | 0.710 ksi | |
Taiwan Sheen Soon Sheenthane® A8230 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00490 GPa | 0.710 ksi | |
Taiwan Sheen Soon Sheenthane® A8361E Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00490 GPa | 0.710 ksi | |
Taiwan Sheen Soon Sheenthane® A8555E Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionPolyether gradeInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00490 GPa | 0.710 ksi | |
Taiwan Sheen Soon Sheenthane® A8600F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00490 GPa | 0.710 ksi | |
Taiwan Sheen Soon Sheenthane® A8630F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00490 GPa | 0.710 ksi | |
Taiwan Sheen Soon Sheenthane® A8631N Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00490 GPa | 0.710 ksi | |
Taiwan Sheen Soon Sheenthane® A8800F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00490 GPa | 0.710 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 70 PHR N990 (MT) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00490 GPa | 0.710 ksi | Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FE 5642 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FE 5642 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |