Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00405 GPa | 0.588 ksi | Original Properties; ASTM D1414 |
Freudenberg Simrit N432 Nitrile Elastomer (NBR) General Purpose; Internal Lubricant. Inferior resistance to ozone, sunlight and natural aging; poor resistance to oxygenated solvents. All testing done on AS568-214 size o-rings |