Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00396 GPa | 0.575 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N330 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00396 GPa | 0.575 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Mistron Vapor Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00396 GPa | 0.575 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N330 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00396 GPa | 0.575 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Mistron Vapor Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00396 GPa | 0.575 ksi | ASTM D638 |
Colorite Polymers 6034 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00396 GPa | 0.575 ksi | ASTM D638 |
Colorite Polymers 6077 Non-Phthalate 77 Series Vinyl Compound Description: The Colorite 77 series is a family of compounds designed for those medical device producers that require the use of a non-phthalate plasticizer that has superior resistance to extractio.. |
|||
100% Modulus | 0.00396 GPa | 0.575 ksi | Perpendicular Flow; ASTM D412 |
Advanced Polymer Alloys DuraGrip™ 6165 TR Thermoplastic Elastomer DuraGrip® DGR6165TR is a translucent thermoplastic elastomer (TPE) formulated for excellent elastic properties and enhanced adhesion to engineered thermoplastics using insert molding, co-injection .. |