Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00372 GPa | 0.540 ksi | |
Spartech E65650 General Purpose PVC First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B.. |
|||
100% Modulus | 0.00372 GPa | 0.540 ksi | Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FT 2350 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FT 2350 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |