Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00362 GPa | 0.525 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.25 PHR Zinc Stearate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00362 GPa | 0.525 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR MBT Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00362 GPa | 0.525 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00362 GPa | 0.525 ksi | ASTM D-638 |
Axiall 8610 Moldings & Extrusions Flexible PVC A high quality, low gravity, clear extrusion and molding compound with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00362 GPa | 0.525 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.25 PHR Zinc Stearate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00362 GPa | 0.525 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR MBT Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00362 GPa | 0.525 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00362 GPa | 0.525 ksi | ASTM D-638 |
Axiall 18660 Moldings & Extrusions Flexible PVC Flame retardant extrusion and molding compound recommended for 105C applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |