Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00343 GPa | 0.497 ksi | |
Taiwan Sheen Soon Sheenthane® A7530 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00343 GPa | 0.497 ksi | |
Taiwan Sheen Soon Sheenthane® A7630 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00343 GPa | 0.497 ksi | |
Taiwan Sheen Soon Sheenthane® A8760 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00343 GPa | 0.497 ksi | |
Taiwan Sheen Soon Sheenthane® A8760F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |