Polymer Property : 100% Modulus = 0.464 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00320 GPa
0.464 ksi
TPE-0153 (ASTM D 412)
Advanced Elastomer Systems Santoprene® 251-80 Thermoplastic Rubber  (discontinued **)
A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b..
100% Modulus 0.00320 GPa
0.464 ksi
ISO 37
Kuraray SEPTON® S2002 Thermoplastic Rubber
SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi..
100% Modulus 0.00320 GPa
0.464 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 6.0 PHR MBTS
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
100% Modulus 0.00320 GPa
0.464 ksi
ASTM D412
C.O.I.M. LARIPUR® LPR7018 Plasticized Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
100% Modulus 0.00320 GPa
0.464 ksi
ISO 37
AlphaGary Evoprene™ 049 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
100% Modulus 0.00320 GPa
0.464 ksi
ISO 37
AlphaGary Evoprene™ Super G 934 SEBS Thermoplastic Elastomer
Evoprene™ Super G compounds are high performance styrene ethylene- butylene styrene based thermoplastic elastomers. Evoprene™ Super G has improved heat resistance and improved recovery properties..
100% Modulus 0.00320 GPa
0.464 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 6.0 PHR MBTS
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
100% Modulus 0.00320 GPa
0.464 ksi
DIN 53504
Lubrizol ESTANE® 58213 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..