Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00293 GPa | 0.425 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N330 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00293 GPa | 0.425 ksi | |
Shin-Etsu Silicones SV-17500U Silicone Rubber SV17500U is one of a series of easy processing, silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendaring. Product Features: This pr.. |
|||
100% Modulus | 0.00293 GPa | 0.425 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N330 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00293 GPa | 0.425 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Hi-Sil 233 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00293 GPa | 0.425 ksi | ASTM D638 |
Colorite Polymers 6284 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00293 GPa | 0.425 ksi | ASTM D-638 |
Axiall 8552 Moldings & Extrusions Flexible PVC A soft extrusion compound recommended for profiles, weatherstrips and sheeting. Also suitable for injection molding.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 201.. |
|||
100% Modulus | 0.00293 GPa | 0.425 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Hi-Sil 233 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00293 GPa | 0.425 ksi | ASTM D412 |
Saint-Gobain Tygon® 2375 Ultra Chemical Resistant Tubing Formulation Tygon® Ultra Chemical Resistant Tubing offers a combination of chemical resistance, clarity and flexibility. Tygon® 2375 replaces 2075.Tygon® Ultra Chemical Resistant Tubing is virtually unaffec.. |