Mechanical Properties Metric English Comments
100% Modulus 0.00240 GPa
0.348 ksi
ISO/R527
Polykemi AB POLYelast TPE Z600A Thermoplastic Elastomer, SEBS-based, Co-injection Grade
Information provided by Polykemi AB
100% Modulus 0.00240 GPa
0.348 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.0 PHR MBT
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
100% Modulus 0.00240 GPa
0.348 ksi
ISO 37
Huntsman AVALON® 60 AE-ESD Thermoplastic Polyurethane
AVALON® ESD range are soft TPUs that deliver the improved bonding strength and mechanical properties required to produce high-quality footwear on roundtable machines – specifically safety sh..
100% Modulus 0.00240 GPa
0.348 ksi
Die C; Cross direction; ASTM D412
Teknor Apex Sarlink® 3160 Thermoplastic Elastomer
A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3160 can be processed by injection molding or extrusion for ap..
100% Modulus 0.00240 GPa
0.348 ksi
Die C; Cross direction; ASTM D412
Teknor Apex Sarlink® 3460 Thermoplastic Elastomer
A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject..
100% Modulus 0.00240 GPa
0.348 ksi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 4155 Thermoplastic Elastomer
A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4155 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re..
100% Modulus 0.00240 GPa
0.348 ksi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 4455 Thermoplastic Elastomer
A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4455 is a low hardness grade possessing exceptional tensile strength, superior compression s..
100% Modulus 0.00240 GPa
0.348 ksi
Conductive CR Conveyor Belt Cover Compound
TIMCAL ENSACO™ 250G Conductive Carbon Black
ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can..
100% Modulus 0.00240 GPa
0.348 ksi
DIN 53504
Lubrizol ESTANE® 5702F3 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
100% Modulus 0.00240 GPa
0.348 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.0 PHR MBT
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
100% Modulus 0.00240 GPa
0.348 ksi
ASTM D412
UBE UBEPOL VCR303 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel..
100% Modulus 0.00240 GPa
0.348 ksi
DIN 53504
Lubrizol ESTANE® 5702F2 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
100% Modulus 0.00240 GPa
0.348 ksi
500 mm/min, measured parallel to flow; ISO 37
AlphaGary Evoprene™ LF 6152 Automotive Thermoplastic Elastomer
Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab..
100% Modulus 0.00240 GPa
0.348 ksi
ASTM D412
Advanced Polymer Alloys Alcryn® 2160 NC Melt Processable Rubber
Alcryn 2100 Series melt-processable rubber (MPR) offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn. The 2100 grades..
100% Modulus 0.00240 GPa
0.348 ksi
ASTM D412
Advanced Polymer Alloys DuraGrip™ 6870 Thermoplastic Elastomer
With its true rubber look and feel, DuraGrip® TPE improves the performance and appearance of virtually any consumer or light industrial product. Its one of the most versatile materials in APAs exte..
100% Modulus 0.00240 GPa
0.348 ksi
Die C; Cross direction; ASTM D412
Teknor Apex Sarlink® 3460N Thermoplastic Elastomer
A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext..
100% Modulus 0.00240 GPa
0.348 ksi
ISO 37
AlphaGary Evoprene™ GC 5690 SEBS Thermoplastic Elastomer
Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can..
100% Modulus 0.00240 GPa
0.348 ksi
500 mm/min, measured parallel to flow; ISO 37