Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00110 GPa | 0.160 ksi | ISO/R527 |
Polykemi AB POLYelast TPE ZS506 Thermoplastic Elastomer, SEBS/SBS-based Information provided by Polykemi AB |
|||
100% Modulus | 0.00110 GPa | 0.160 ksi | press cure 11 min./160ºC |
TSE Industries Millathane® 26 Millable Polyether Urethane for Food Contact Applications Millathane 26 is a polyether polyurethane rubber compliant with the United States Code of Federal Regulations*, Title 21 parts 177.1680 and 177.2600. This polyurethane rubber is designed for food co.. |
|||
100% Modulus | 0.00110 GPa | 0.160 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Friction Compound MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00110 GPa | 0.160 ksi | |
Mearthane Durethaneâ„¢ F DF-245A Closed Cell Foam Polyurethane TDI backbone: ester.Shore 00 Hardness: 90Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient.. |
|||
100% Modulus | 0.00110 GPa | 0.160 ksi | |
Mearthane Durethaneâ„¢ F DF-255A Closed Cell Foam Polyurethane TDI backbone: ester.Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient of friction, abrasio.. |
|||
100% Modulus | 0.00110 GPa | 0.160 ksi | press cure 11 min./160ºC |
TSE Industries Millathane® 26 Millable Polyether Urethane for Food Contact Applications Millathane 26 is a polyether polyurethane rubber compliant with the United States Code of Federal Regulations*, Title 21 parts 177.1680 and 177.2600. This polyurethane rubber is designed for food co.. |
|||
100% Modulus | 0.00110 GPa | 0.160 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Friction Compound MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00110 GPa | 0.160 ksi | ASTM D412 |
Elastocon TPE Technologies Elastocon® 8138B Thermoplastic Elastomer Elastocon® 8138B is a black thermoplastic elastomer compound formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8138B is well suited for consumer.. |
|||
100% Modulus | 0.00110 GPa | 0.160 ksi | High-K Stress Control Tube; ASTM D412 |
3M 7620-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl.. |
|||
100% Modulus | 0.00110 GPa | 0.160 ksi | High-K Stress Control Tube; ASTM D412 |
3M 7620-T Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-Tand 7690-T Series, contain one-piece, non-skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 for indo.. |
|||
100% Modulus | 0.00110 GPa | 0.160 ksi | High-K Stress Control Tube; ASTM D412 |
3M 7650-S-HSG Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7650-S-HSG and 7660-S-HSG Series, are designed for applications requiring a high-ampacity ground. Each kit contains one-piece, skirt.. |
|||
100% Modulus | 0.00110 GPa | 0.160 ksi | High-K Stress Control Tube; ASTM D412 |
3M 7660-S Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7640-S, 7650-S and 7660-S Series, contains one-piece, skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 fo.. |
|||
100% Modulus | 0.00110 GPa | 0.160 ksi | High-K Stress Control Tube; ASTM D412 |
3M 7660-S-HSG Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7650-S-HSG and 7660-S-HSG Series, are designed for applications requiring a high-ampacity ground. Each kit contains one-piece, skirt.. |
|||
100% Modulus | 0.00110 GPa | 0.160 ksi | High-K Stress Control Tube; ASTM D412 |
3M 7680-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl.. |
|||
100% Modulus | 0.00110 GPa | 0.160 ksi | High-K Stress Control Tube; ASTM D412 |
3M 7690-T Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-Tand 7690-T Series, contain one-piece, non-skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 for indo.. |
|||
100% Modulus | 0.00110 GPa | 0.160 ksi | ISO 37 |
AlphaGary Evoprene™ 019 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
100% Modulus | 0.00110 GPa | 0.160 ksi | Press cure 10 Minutes @ 177°C, Post Cure 16 Hours @ 232°C; ASTM D412 |
3M Dyneon™ PFE 60Z Perfluoroelastomer Dyneon™ PFE 60 Z is a technically advanced peroxide curable perfluoroelastomer, designed to meet the challenges of demanding sealing applications. It’s fully fluorinated back bone structure provid.. |
|||
100% Modulus | 0.00110 GPa | 0.160 ksi | High-K Stress Control Tube; ASTM D412 |
3M 7640-S Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7640-S, 7650-S and 7660-S Series, contains one-piece, skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 fo.. |
|||
100% Modulus | 0.00110 GPa | 0.160 ksi | High-K Stress Control Tube; ASTM D412 |
3M 7650-S Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7640-S, 7650-S and 7660-S Series, contains one-piece, skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 fo.. |
|||
100% Modulus | 0.00110 GPa | 0.160 ksi | High-K Stress Control Tube; ASTM D412 |
3M 7690-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl.. |
|||
100% Modulus | 0.00110 GPa | 0.160 ksi | ISO 37 |
AlphaGary Evoprene™ GC 5696 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |
|||
100% Modulus | 0.00110 GPa | 0.160 ksi | ISO 37 |
AlphaGary Evoprene™ Super G 947 SEBS Thermoplastic Elastomer Evoprene™ Super G compounds are high performance styrene ethylene- butylene styrene based thermoplastic elastomers. Evoprene™ Super G has improved heat resistance and improved recovery properties.. |