Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.000896 GPa | 0.130 ksi | DCBP Cure |
Shin-Etsu Silicones KE-541U Silicone Rubber KE541U is one of a series of easy processing, general purpose grade silicone rubber bases. It can be used in a variety of applications requiring finishing by molding or extruding with extending fill.. |
|||
100% Modulus | 0.000896 GPa | 0.130 ksi | ASTM D 412 |
CPT C-Flex® R70-091 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
100% Modulus | 0.000896 GPa | 0.130 ksi | Silicone Rubber Insulator; ASTM D412 |
3M 7620-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl.. |
|||
100% Modulus | 0.000896 GPa | 0.130 ksi | Silicone Rubber Insulator; ASTM D412 |
3M 7620-T Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-Tand 7690-T Series, contain one-piece, non-skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 for indo.. |
|||
100% Modulus | 0.000896 GPa | 0.130 ksi | Silicone Rubber Insulator; ASTM D412 |
3M 7660-S Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7640-S, 7650-S and 7660-S Series, contains one-piece, skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 fo.. |
|||
100% Modulus | 0.000896 GPa | 0.130 ksi | Silicone Rubber Insulator; ASTM D412 |
3M 7680-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl.. |
|||
100% Modulus | 0.000896 GPa | 0.130 ksi | Silicone Rubber Insulator; ASTM D412 |
3M 7690-T Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-Tand 7690-T Series, contain one-piece, non-skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 for indo.. |
|||
100% Modulus | 0.000896 GPa | 0.130 ksi | Silicone Rubber Insulator; ASTM D412 |
3M 7640-S Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7640-S, 7650-S and 7660-S Series, contains one-piece, skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 fo.. |
|||
100% Modulus | 0.000896 GPa | 0.130 ksi | Silicone Rubber Insulator; ASTM D412 |
3M 7650-S Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7640-S, 7650-S and 7660-S Series, contains one-piece, skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 fo.. |
|||
100% Modulus | 0.000896 GPa | 0.130 ksi | Silicone Rubber Insulator; ASTM D412 |
3M 7690-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl.. |