Mechanical Properties Metric English Comments
100% Modulus 0.0128 - 0.0152 GPa
1.85 - 2.20 ksi
Secant; Conditioned 7 days at RT/50% RH; ASTM D638
AdvanSource Biomaterials ChronoFlex® C 55D Biodurable Medical Grade Polyurethane
ChronoFlex® C is a family of premium polycarbonate aromatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® C medical-grade elastome..